FraMCoS 3

This text briefly introduces the content in the page.

Delamination Criterion for Concrete Beams Retrofitted with FRP Laminates

fiber-reinforced plastics (FRP) to infrastructure has become an attractive choice of structural ·and retrofit methods worldwide. load capacity concrete girders can be enhanced by the application of face of the element, but of these systems and can generally ‘V’…., • .., …… _…._ …. ;;:;…. concrete substrate. debonding mechanism is a local by stress intensities

Delamination Failure in Concrete Beams Retrofitted with a Bonded Plate

Concrete beams can be retrofitted by bonding a steel or composite plate to its bottom. The failure of such members is usually due to the delamination of the plate from the beam. Delamination can occur either at the end of the reinforcing plate or at the location of a crack in the concrete beam. This

Plate End Shear Design for External CFRP Laminates

In the design of externally bonded reinforcement, the anchoring design is extremely important, because failure is very often initiated in the end zones. Expressions for the anchoring capacity in both the serviceability limit state and the ultimate limit state are derived from the classical differential equation of Volkersen. Therefore non-linear concrete properties, describing the pre-

Materials and Design Considerations in FRP Rehabilitation of Concrete Structures

Fiber reinforced polymer matrix composites are increasingly being considered for use in repair, strengthening and retrofit of concrete structures. The technology is now at a point where its future acceptance will depend primarily on the availability of validated design guidelines based on accepted performance criteria, and on the economic competitiveness of these technologies as compared

Characterization of Interface Fracture Behavior in Repaired Concrete Infrastructures

Usually repair systems can be divided into three different phases of materials — repaired substrate phase, repair material phase and the interface phase between substrate and repair material. Each phase of material has to have its own role in the system for durable repair. Among the three phases, the interface phase especially has the most

LEFM Prediction and Repair Strategy for Crack Extension due to Corrosion of Reinforcement

In order to repair cracks of concrete, the causes of cracking have been intensively studied and can be identified mostly in inspected structures. One of critical cracks is known to result from corrosion of steel reinforcement in concrete. Due to expansion of corrosive products, tensile cracks of various patterns are nucleated around rebars. Initiation and

Evaluation of Bond Behavior at the Interface Between Two Different Concretes

Bond performance of a deformed steel bar lying at the interface between old and new concretes was examined using both experimental and numeri- cal procedures. In the experimental study, fifty-seven Schmidt-Thro type specimens were tested to study the influence of concrete strength (30 MPa – 100 MPa) and interface conditions on the side split type

Fracture Mechanics Study of Concrete Beams Reinforced with FRP Sheets by a Moment Tensor Analysis of Acoustic Emission

Center notched concrete beams reinforced with carbon and glass fiber rein- forced plastic sheets were subjected to three-point flexure loading. Con- ventional AE parameter analysis showed that the beginning of continuous occurrence and exponentially increment of AE activities corresponds to the critical load at which the crack initiates at the notch tip. The critical stress

Fracture and Fatigue Strength of Slabs Repaired with D-Rap Method

Reinforced concrete slabs on the steel girders of old highway bridge get damage occasionally. Various repairing methods of damaged deck slab have been developed and adopted in site. A new repairing method of the damaged RC slabs named D-RAP method was developed where double layered pre-fabricated panels were glued on the top surface of concrete

Probabilistic Study on the Tensile Strength of Multiple-FRP Tendons

This study analyzed the failure load of FRP multiple-tendon systems having a design strength of 130 tf, by using the weakest link model and the Monte Carlo method to examine the tensile strength characteristics of the systems. It was found that the mean value and the standard de- viation of a tension test could be

Do you want to boost your business today?