FraMCoS 11 2023 Bangalore, India

A new perspective on crack instability of spalling concrete in fire

Explosive spalling keeps being one of the main open issues concerning the fire safety of concrete structures. Though it is recognized that cracks in the exposed cover can be triggered by the combined effect of thermal stress and pore pressure,…

First page of: A new perspective on crack instability of spalling concrete in fire
Year 2023
Downloads 1
File Size 590 KB
Download PDF (590 KB)

Abstract

Explosive spalling keeps being one of the main open issues concerning the fire safety of concrete structures. Though it is recognized that cracks in the exposed cover can be triggered by the combined effect of thermal stress and pore pressure, the energy source and the mechanism behind the violent projection of fragments are not yet fully understood. Nonetheless, the huge thermal 2 energy accumulated in the hot cover (in the order of 500kJ/m in a 1mm thick layer) has a high potential to drive dynamic fracturing, provided that water vaporization could quickly convert it into mechanical work. To make this possible, flash vaporization of a significant amount of water should take place in a sub-millimetre layer facing the opening crack (since vapour diffusion time goes with the path length squared). To validate this new perspective, a special setup was developed where concrete disks (D=100mm, thickness=60mm) were heated on the two opposite faces, so to instate a thermo-hygral transient similar to the concrete cover exposed to fire, while keeping negligible the contribution of thermal stress. A crack is triggered in the sample mid-plane by the high thermal dilation of a polymeric insert (a PTFE ring) embedded in the sample. FEM analyses were performed to optimize the specimen shape and to adjust the insert thickness to control the temperature at which the crack develops a critical opening. Remarkably unstable blasts were observed in high-performance concrete samples, during which the relative acceleration of the two splitting halves was monitored via optical sensors. The results showed that pressure not far from the saturation value quickly develops in the opening crack. Continuous monitoring of the specimen mass also allowed assessing the amount of vaporized water entailed by the process. Tests on pre-dried samples exhibited a milder blast or even a stable propagation of the crack. In summary, this study is expected to cast new light on the fundamental mechanism behind the explosive spalling phenomenon.