An experimental study on mode II fracture of the joint-grouting material between two blocks of the concrete dam is carried out by using the double-edge notched mode II specimens. In consideration of the difficulty in determination of the critical load,…

First page of: Experimental determination of mode II fracture toughness KIIc for joint grouting material by using electric properties
Year 2010
File Size 946 KB
Download PDF (946 KB)

Abstract

An experimental study on mode II fracture of the joint-grouting material between two blocks of the concrete dam is carried out by using the double-edge notched mode II specimens. In consideration of the difficulty in determination of the critical load, the electric property of the joint-grouting material is applied to obtain the critical load of mode II fracture for double-edge notched specimen with preformed joint in the pre- sent test. It is found that the KIIc of the joint-grouting material is dependent on the specimen depth and width, and is independent of initial crack to depth ratio. The experimental results also show that electric resistance increases with the increase of the measured load and displacement, and the behavior of electric resistance of joint-grouting material can be used to determine the critical mode II fracture load which is a basis to ascertain KIIc values of the joint-grouting material using the double-edge specimen. 1 INSTRUCTIONS been applied to monitor mode II fracture process of double-edge specimens in the experiment. During the construction of bulk concrete structures, grouting is always applied between the construction joints to make the structure as a whole to undertake 2 EXPERIMENTAL STUDY applied load after temperature and deformation of concrete stabilize. However, a relative weak section 2.1 Double-edge mode II specimens forms at the joint-grouting interface of dam, where Figure 1 shows the model of rectangle double-edge mode II fracture is likely to occur under seismic ac- notched plate. Middle of the plate is the ligament tion or thermal stress. Therefore, the characteristics which stands for grouting joint.